CC483K

bushing

A technical illustration of the product with dimensions of the material CC483K from the material Bronze in the shape bushing
  • Form bushing
  • Material Bronze
  • Material CC483K
  • Material chemically EN 573-3 Cu Sn 12

No product available for your selection.

An image of the material CC483K from the material Bronze in the shape bushing
A technical illustration of the product of the material CC483K from the material Bronze in the shape bushing

Information about the material

  • Aviation
    Aviation No
  • Chemical specifications
    Al (from) 0.01
    Al (to) 0.01
    Cu (from) 85
    Cu (to) 88.5
    Fe (from) 0.2
    Fe (to) 0.2
    Mn (from) 0.2
    Mn (to) 0.2
    Ni (to) 2
    P (to) 0.6
    Pb (to) 0.7
    S (from) 0.05
    S (to) 0.05
    Sb (from) 0.15
    Sb (to) 0.15
    Si (from) 0.01
    Si (to) 0.01
    Sn (from) 11
    Sn (to) 13
    Zn (from) 0.5
    Zn (to) 0.5
  • Food industry
    suitable according to DIN EN 602 No
  • Material
    Material chemically EN 573-3 Cu Sn 12
    Material no CC483K
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 17.8 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 200°C 18.1 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 300°C 18.5 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 400°C 18.9 K⁻¹10⁻⁶
    Density 8.72 g/cm³
    Modulus of elasticity at 100°C 95 GPa
    Modulus of elasticity at 20°C 97 GPa
    Modulus of elasticity at 200°C 92 GPa
    Modulus of elasticity at 300°C 89 GPa
    Modulus of elasticity at 400°C 85 GPa
    Specific electrical conductivity at 20°C 6.2 m/Ω*mm²
    Specific electrical conductivity at 200°C 5.3 m/Ω*mm²
    Specific electrical resistance at 20°C 0.161 Ω*mm²/m
    Specific electrical resistance at 200°C 0.189 Ω*mm²/m
    Specific heat at 100°C 0.385 J/(kg·K)
    Specific heat at 20°C 0.376 J/(kg·K)
    Specific heat at 200°C 0.395 J/(kg·K)
    Thermal conductivity at 100°C 62 W/m*K
    Thermal conductivity at 20°C 55 W/m*K
    Thermal conductivity at 200°C 70 W/m*K
  • Soldering
    Brazing 3
    Soft soldering 1
  • Welding
    Gas 3
    MIG 3
    Resistance spot welding 2
    TIG 3
  • Aviation
    Aviation No
  • Chemical specifications
    Al (from) 0.01
    Al (to) 0.01
    Cu (from) 85
    Cu (to) 88.5
    Fe (from) 0.2
    Fe (to) 0.2
    Mn (from) 0.2
    Mn (to) 0.2
    Ni (to) 2
    P (to) 0.6
    Pb (to) 0.7
    S (from) 0.05
    S (to) 0.05
    Sb (from) 0.15
    Sb (to) 0.15
    Si (from) 0.01
    Si (to) 0.01
    Sn (from) 11
    Sn (to) 13
    Zn (from) 0.5
    Zn (to) 0.5
  • Food industry
    suitable according to DIN EN 602 No
  • Material
    Material chemically EN 573-3 Cu Sn 12
    Material no CC483K
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 17.8 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 200°C 18.1 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 300°C 18.5 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 400°C 18.9 K⁻¹10⁻⁶
    Density 8.72 g/cm³
    Modulus of elasticity at 100°C 95 GPa
    Modulus of elasticity at 20°C 97 GPa
    Modulus of elasticity at 200°C 92 GPa
    Modulus of elasticity at 300°C 89 GPa
    Modulus of elasticity at 400°C 85 GPa
    Specific electrical conductivity at 20°C 6.2 m/Ω*mm²
    Specific electrical conductivity at 200°C 5.3 m/Ω*mm²
    Specific electrical resistance at 20°C 0.161 Ω*mm²/m
    Specific electrical resistance at 200°C 0.189 Ω*mm²/m
    Specific heat at 100°C 0.385 J/(kg·K)
    Specific heat at 20°C 0.376 J/(kg·K)
    Specific heat at 200°C 0.395 J/(kg·K)
    Thermal conductivity at 100°C 62 W/m*K
    Thermal conductivity at 20°C 55 W/m*K
    Thermal conductivity at 200°C 70 W/m*K
  • Soldering
    Brazing 3
    Soft soldering 1
  • Welding
    Gas 3
    MIG 3
    Resistance spot welding 2
    TIG 3

1 very good
2 good
3 moderate
4 poor
5 unsuited