EN AW-2007
hexagon bar drawn
- Form hexagon bar drawn
 - Material Aluminum
 - Material EN AW-2007
 - Material chemically EN 573-3 AlCu4PbMgMn
 - DIN 3.1645
 
            
            
            
            | Aviation | No | 
| Be (from) | 0 | 
| Be (to) | 0 | 
| Bi (to) | 0,2 | 
| Co (from) | 0 | 
| Co (to) | 0 | 
| Cr (to) | 0,1 | 
| Cu (from) | 3,3 | 
| Cu (to) | 4,6 | 
| Fe (to) | 0,8 | 
| Mg (from) | 0,4 | 
| Mg (to) | 1,8 | 
| Mn (from) | 0,5 | 
| Mn (to) | 1 | 
| Ni (to) | 0,2 | 
| Other | 0,10 | 
| Pb (from) | 0,8 | 
| Pb (to) | 1,5 | 
| Rest | Aluminium | 
| Si (to) | 0,8 | 
| Sn (to) | 0,8 | 
| Ti (to) | 0,2 | 
| Total | 0,30 | 
| Zn (to) | 0,8 | 
| Anodise - decorative | 5 | 
| Anodising - protective anodising | 4,5 | 
| Chromating | 2 | 
| Cleaning / degreasing | 2 | 
| Hard anodising | 3 | 
| Phosphating | 2 | 
| Pickling | 2 | 
| Shining | 4,5 | 
| Normal atmosphere | 4,5 | 
| Seawater atmosphere | 4,5 | 
| Laser cutting | 4,5 | 
| Plasma cutting | 4,5 | 
| Sawing | 1 | 
| Shear cutting | 2 | 
| Waterjet cutting | 1 | 
| suitable according to DIN EN 602 | No | 
| Bending | 4,5 | 
| Extruding | 4 | 
| Press conditions | O/H111 | 
| Upsetting (Conditional) | 4,5 | 
| Heating time max. | 2 h | 
| Heating time min. | 1 h | 
| Annealing temperature max. | 420 °C | 
| Annealing temperature min. | 380 °C | 
| Cooling conditions | 
                                Cooling conditions 30°C/h to  250°C, below 250°C in air  | 
                        
| Cold ageing max. | 8 d | 
| Cold ageing min. | 5 d | 
| Heat ageing min. | 16 h | 
| Heating temperature min. | 160 °C | 
| Quenching | water to 65°C | 
| Solution annealing max. | 490 °C | 
| Solution annealing min. | 480 °C | 
| dimensional stability | 2 | 
| Eroding | 1 | 
| Etching | 2 | 
| hardened | 1 | 
| Photo etching | 2 | 
| Colorcode | Signalschwarz (RAL 9004) | 
| Material chemically EN 573-3 | AlCu4PbMgMn | 
| DIN | 3,1645 | 
| DIN (old designation) | Al Cu Mg Pb | 
| France AFNOR | - | 
| Italy UNI | 9002/8 | 
| Norway | 17.110 | 
| Spain | - | 
| Sweden | - | 
| United Kingdom BS | - | 
| Blasting | 1 | 
| Brushing | 2 | 
| Grinding | 2 | 
| Polishing | 3 | 
| Galvanising | 2 | 
| Nickel coating | 2 | 
| Thermal spraying | 4,5 | 
| Enamelling | 4,5 | 
| Laminating | 2 | 
| Painting / Coating | 4 | 
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ | 
| Density | 2.85 g/cm³ | 
| Electrical conductivity max. | 22 m/Ω*mm² | 
| Electrical conductivity min. | 18 m/Ω*mm² | 
| Modulus of elasticity | 72.5 GPa | 
| Shear modulus | 27.3 GPa | 
| Specific heat | 860 J/(kg·K) | 
| Thermal conductivity max. | 160 W/m*K | 
| Thermal conductivity min. | 130 W/m*K | 
| Brazing | 5 | 
| Brazing with flux | 5 | 
| Friction soldering | 4,5 | 
| Friction stir welding | 5 | 
| Friction welding | 5 | 
| Laser | 5 | 
| Plasma | 5 | 
                            1 very good
                            2 good
                            3 moderate
                            4 poor
                            5 unsuited
                            0 Not specified