EN AW-6060
half-round bar
- Form half-round bar
- Material Aluminum
- Material EN AW-6060
- Material chemically EN 573-3 Al Mg Si
- DIN 3.3206
Aviation | No |
Be (from) | 0 |
Be (to) | 0 |
Co (from) | 0 |
Co (to) | 0 |
Cr (to) | 0.05 |
Cu (to) | 0.1 |
Fe (from) | 0.1 |
Fe (to) | 0.3 |
Mg (from) | 0.35 |
Mg (to) | 0.6 |
Mn (to) | 0.1 |
Other | 0,05 |
Rest | Aluminium |
Si (from) | 0.3 |
Si (to) | 0.6 |
Ti (to) | 0.1 |
Total | 0,15 |
Zn (to) | 0.15 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
Anodise - decorative | 1.5 |
Anodising - protective anodising | 1 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 3 |
special anodising quality EQ | 1 |
Normal atmosphere | 1 |
Seawater atmosphere | 2 |
Laser cutting | 3 |
Plasma cutting | 2 |
Sawing | 2 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 3 |
Bending delivery conditions | T3 · T4 |
Drop forging | 1 |
Extruding | 1 |
Impact extrusion | 2 |
Impact extrusion conditions | O |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 400 °C |
Annealing temperature min. | 360 °C |
Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
Cold ageing condition | danach |
Cold ageing max. | 8 d |
Cold ageing min. | 5 d |
Heat ageing max. | 16 h |
Heat ageing min. | 4 h |
Heating temperature max. | 190 °C |
Heating temperature min. | 155 °C |
Quenching | water ∙ air |
Solution annealing max. | 540 °C |
Solution annealing min. | 525 °C |
Eroding | 1 |
Etching | 2 |
hardened | 2 |
Photo etching | 2 |
soft annealed | 3.5 |
Colorcode | neutral |
Material chemically EN 573-3 | Al Mg Si |
DIN | 3.3206 |
DIN (old designation) | Al Mg Si0,5 |
France AFNOR | A-GS |
Italy UNI | 9006/1 |
Norway | 17,310 |
Spain | L-3442 |
Sweden | 144,103 |
Blasting | 1 |
Brushing | 3 |
Dessinating | 1 |
Grinding | 3 |
Polishing | 1 |
Galvanising | 2 |
Nickel coating | 2 |
Thermal spraying | 4 |
Enamelling | 4 |
Laminating | 2 |
Painting / Coating | 1 |
Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 24.5 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 25.6 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 21.8 K⁻¹10⁻⁶ |
Density | 2.7 g/cm³ |
Electrical conductivity max. | 38 m/Ω*mm² |
Electrical conductivity min. | 34 m/Ω*mm² |
Modulus of elasticity | 69.5 GPa |
Shear modulus | 26.1 GPa |
Specific heat | 898 J/(kg·K) |
Thermal conductivity max. | 220 W/m*K |
Thermal conductivity min. | 200 W/m*K |
Brazing | 2 |
Brazing with flux | 2 |
Friction soldering | 1 |
Soft soldering | 2 |
Soft soldering with flux | 1 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
TIG | 2 |
welding additives |
|
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified