FORMODAL®019 elox
circular blank
- Form circular blank
- Material Aluminum
- Material FORMODAL®019 elox
- Material chemically EN 573-3 AA 5754
Aviation | No |
Cr (to) | 0.3 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 2.6 |
Mg (to) | 3.6 |
Mn (to) | 0.5 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.2 |
Anodise - decorative | 2 |
Anodising - protective anodising | 1 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 4 |
Deep drawing (conditional) | 5 |
Drop forging | 1 |
Extruding | 1 |
Impact extrusion | 4 |
Open die forging | 1 |
Press | 4 |
Upsetting (Conditional) | 4 |
Annealing temperature min. | 345 °C |
dimensional stability | 1 |
Eroding | 2 |
Material chemically EN 573-3 | AA 5754 |
France AFNOR | - |
Italy UNI | - |
Norway | - |
Spain | - |
Sweden | - |
United Kingdom BS | - |
Polishing | 2 |
Painting / Coating | 3 |
Coefficient of thermal expansion from 20 to 100°C (typical) | 23.9 K⁻¹10⁻⁶ |
Density (typical) | 2.67 g/cm³ |
Electrical conductivity max. (typical) | 23 m/Ω*mm² |
Electrical conductivity min. (typical) | 20 m/Ω*mm² |
Modulus of elasticity (typical) | 70 GPa |
Specific heat (typical) | 900 J/(kg·K) |
Thermal conductivity max. (typical) | 160 W/m*K |
Thermal conductivity min. (typical) | 130 W/m*K |
Brazing | 4 |
Brazing with flux | 5 |
Friction soldering | 3 |
Soft soldering with flux | 5 |
Gas | 2 |
MIG | 1 |
Resistance spot welding | 3 |
TIG | 1 |
welding additives |
|
1 very good
2 good
3 moderate
4 poor
5 unsuited