CC333G

bushing

A technical illustration of the product with dimensions of the material CC333G from the material Bronze in the shape bushing
  • Form bushing
  • Material Bronze
  • Material CC333G
  • Material chemically EN 573-3 Bronze Cu Al10 Fe5 Ni5-C

No product available for your selection.

An image of the material CC333G from the material Bronze in the shape bushing
A technical illustration of the product of the material CC333G from the material Bronze in the shape bushing

Areas of application

Hot steam fittings

Manifold heads and reversing bottoms in apparatus engineering and petrochemistry, pump casings, impellers, shafts, protective sleeves
pipes, compressors

seawater-cooled superheaters

Areas of application

Lock parts, propeller hubs, blades, bonnets, shafts

Stern tubes, anchor nozzles, screws

Distilling apparatus, boilers

Areas of application

Tube end plates

Water and oil coolers, water chambers

Desalination plants, salt boiling plants

Areas of application

Agitators, pickling baskets, heat exchangers

Turbine parts, guide vanes, distributor fans

Toothed and worm wheels

Areas of application

Strips, pressure nuts, joints

Bearing bushes, collector rings

Deep-drawing tools, profile rollers

Areas of application

Moulds and cores for plastics processing

Parts for glass processing and for the electrical and electronic industry, spark-proof tools, etc.

Features of this material

  • excellent corrosion resistance

Information about the material

  • Aviation
    Aviation No
  • Chemical specifications
    Al footnote reference 2
    Al (from) 8.5
    Al (to) 10.5
    Bi (from) 0.01
    Bi (to) 0.01
    Cr (from) 0.05
    Cr (to) 0.05
    Cu (from) 76
    Cu (to) 83
    Fe footnote reference 1
    Fe (from) 4
    Fe (to) 5.5
    Mg (from) 0.05
    Mg (to) 0.05
    Mn (to) 3
    Ni (from) 4
    Ni (to) 6
    Si (from) 0.1
    Si (to) 0.01
    Sn (from) 0.1
    Sn (to) 0.1
    Zn (from) 0.5
    Zn (to) 0.5

    1) Für Kokillenguss muss der Mindestgehalt bei Blockmetallen und
    Gussstücken 3,0 % betragen, und der Mindestnickelgehalt muss
    3,7 % betragen.


    2) Bei Korrosionsbeanspruchung soll der Al-Gehalt kleiner/gleich
    8,5 + Ni/2 betragen. 

  • Food industry
    suitable according to DIN EN 602 No
  • Material
    Material chemically EN 573-3 Bronze Cu Al10 Fe5 Ni5-C
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 16.3 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 200°C 16.5 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 300°C 17.1 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 400°C 17.8 K⁻¹10⁻⁶
    Density 7.6 g/cm³
    Modulus of elasticity at 100°C 120 GPa
    Modulus of elasticity at 20°C 124 GPa
    Modulus of elasticity at 200°C 115 GPa
    Modulus of elasticity at 300°C 108 GPa
    Specific electrical conductivity at 20°C 4.6 m/Ω*mm²
    Specific electrical conductivity at 200°C 4.3 m/Ω*mm²
    Specific electrical resistance at 20°C 0.215 Ω*mm²/m
    Specific electrical resistance at 200°C 0.233 Ω*mm²/m
    Specific heat at 20°C 0.42 J/(kg·K)
    Thermal conductivity at 100°C 59 W/m*K
    Thermal conductivity at 20°C 51 W/m*K
    Thermal conductivity at 200°C 66 W/m*K
  • Soldering
    Brazing 3
    Soft soldering 4
  • Welding
    Gas 6
    MIG 1
    Resistance spot welding 2
    TIG 1
  • Aviation
    Aviation No
  • Chemical specifications
    Al footnote reference 2
    Al (from) 8.5
    Al (to) 10.5
    Bi (from) 0.01
    Bi (to) 0.01
    Cr (from) 0.05
    Cr (to) 0.05
    Cu (from) 76
    Cu (to) 83
    Fe footnote reference 1
    Fe (from) 4
    Fe (to) 5.5
    Mg (from) 0.05
    Mg (to) 0.05
    Mn (to) 3
    Ni (from) 4
    Ni (to) 6
    Si (from) 0.1
    Si (to) 0.01
    Sn (from) 0.1
    Sn (to) 0.1
    Zn (from) 0.5
    Zn (to) 0.5

    1) Für Kokillenguss muss der Mindestgehalt bei Blockmetallen und
    Gussstücken 3,0 % betragen, und der Mindestnickelgehalt muss
    3,7 % betragen.


    2) Bei Korrosionsbeanspruchung soll der Al-Gehalt kleiner/gleich
    8,5 + Ni/2 betragen. 

  • Food industry
    suitable according to DIN EN 602 No
  • Material
    Material chemically EN 573-3 Bronze Cu Al10 Fe5 Ni5-C
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 16.3 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 200°C 16.5 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 300°C 17.1 K⁻¹10⁻⁶
    Coefficient of thermal expansion from 20 to 400°C 17.8 K⁻¹10⁻⁶
    Density 7.6 g/cm³
    Modulus of elasticity at 100°C 120 GPa
    Modulus of elasticity at 20°C 124 GPa
    Modulus of elasticity at 200°C 115 GPa
    Modulus of elasticity at 300°C 108 GPa
    Specific electrical conductivity at 20°C 4.6 m/Ω*mm²
    Specific electrical conductivity at 200°C 4.3 m/Ω*mm²
    Specific electrical resistance at 20°C 0.215 Ω*mm²/m
    Specific electrical resistance at 200°C 0.233 Ω*mm²/m
    Specific heat at 20°C 0.42 J/(kg·K)
    Thermal conductivity at 100°C 59 W/m*K
    Thermal conductivity at 20°C 51 W/m*K
    Thermal conductivity at 200°C 66 W/m*K
  • Soldering
    Brazing 3
    Soft soldering 4
  • Welding
    Gas 6
    MIG 1
    Resistance spot welding 2
    TIG 1

1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified