CC483K
cast plate - all sides sawn
- Form cast plate - all sides sawn
- Material Bronze
- Material CC483K
- Material chemically EN 573-3 Cu Sn 12
Aviation | No |
Al (from) | 0.01 |
Al (to) | 0.01 |
Cu (from) | 85 |
Cu (to) | 88.5 |
Fe (from) | 0.2 |
Fe (to) | 0.2 |
Mn (from) | 0.2 |
Mn (to) | 0.2 |
Ni (to) | 2 |
P (to) | 0.6 |
Pb (to) | 0.7 |
S (from) | 0.05 |
S (to) | 0.05 |
Sb (from) | 0.15 |
Sb (to) | 0.15 |
Si (from) | 0.01 |
Si (to) | 0.01 |
Sn (from) | 11 |
Sn (to) | 13 |
Zn (from) | 0.5 |
Zn (to) | 0.5 |
suitable according to DIN EN 602 | No |
Material chemically EN 573-3 | Cu Sn 12 |
Material no | CC483K |
Coefficient of thermal expansion from 20 to 100°C | 17.8 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 18.1 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 18.5 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 400°C | 18.9 K⁻¹10⁻⁶ |
Density | 8.72 g/cm³ |
Modulus of elasticity at 100°C | 95 GPa |
Modulus of elasticity at 20°C | 97 GPa |
Modulus of elasticity at 200°C | 92 GPa |
Modulus of elasticity at 300°C | 89 GPa |
Modulus of elasticity at 400°C | 85 GPa |
Specific electrical conductivity at 20°C | 6.2 m/Ω*mm² |
Specific electrical conductivity at 200°C | 5.3 m/Ω*mm² |
Specific electrical resistance at 20°C | 0.161 Ω*mm²/m |
Specific electrical resistance at 200°C | 0.189 Ω*mm²/m |
Specific heat at 100°C | 0.385 J/(kg·K) |
Specific heat at 20°C | 0.376 J/(kg·K) |
Specific heat at 200°C | 0.395 J/(kg·K) |
Thermal conductivity at 100°C | 62 W/m*K |
Thermal conductivity at 20°C | 55 W/m*K |
Thermal conductivity at 200°C | 70 W/m*K |
Brazing | 3 |
Soft soldering | 1 |
Gas | 3 |
MIG | 3 |
Resistance spot welding | 2 |
TIG | 3 |
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified