Red brass CC493K
Round bar
 
                                    - Form Round bar
- Material Bronze
- Material Red brass CC493K
- Material chemically EN 573-3 CuSn7ZnPb
 
             
             
                                     
             
            | Aviation | No | 
| Al (to) | 0,01 | 
| Cu (from) | 81 | 
| Cu (to) | 85 | 
| Fe (to) | 0,2 | 
| Ni (to) | 2 | 
| P (to) | 0,1 | 
| Pb (from) | 5 | 
| Pb (to) | 8 | 
| S (to) | 0,1 | 
| Sb (to) | 0,3 | 
| Si (to) | 0,01 | 
| Sn (from) | 6 | 
| Sn (to) | 8 | 
| Zn (from) | 2 | 
| Zn (to) | 5 | 
| suitable according to DIN EN 602 | No | 
| Material chemically EN 573-3 | CuSn7ZnPb | 
| Material no | CC493K (2.1090.01, .03, .04) | 
| Coefficient of thermal expansion from 20 to 100°C | 18 K⁻¹10⁻⁶ | 
| Coefficient of thermal expansion from 20 to 200°C | 18.3 K⁻¹10⁻⁶ | 
| Coefficient of thermal expansion from 20 to 300°C | 18.7 K⁻¹10⁻⁶ | 
| Coefficient of thermal expansion from 20 to 400°C | 19.1 K⁻¹10⁻⁶ | 
| Density | 8.83 g/cm³ | 
| Modulus of elasticity at 100°C | 94 GPa | 
| Modulus of elasticity at 20°C | 101 GPa | 
| Modulus of elasticity at 200°C | 88 GPa | 
| Modulus of elasticity at 300°C | 85 GPa | 
| Specific electrical conductivity at 20°C | 7.5 m/Ω*mm² | 
| Specific electrical conductivity at 200°C | 6.5 m/Ω*mm² | 
| Specific electrical resistance at 20°C | 0.133 Ω*mm²/m | 
| Specific electrical resistance at 200°C | 0.154 Ω*mm²/m | 
| Specific heat at 100°C | 0.39 J/(kg·K) | 
| Specific heat at 20°C | 0.38 J/(kg·K) | 
| Specific heat at 200°C | 0.4 J/(kg·K) | 
| Thermal conductivity at 100°C | 72 W/m*K | 
| Thermal conductivity at 20°C | 64 W/m*K | 
| Thermal conductivity at 200°C | 82 W/m*K | 
| Brazing | 3 | 
| Soft soldering | 2 | 
| Gas | 6 | 
                            1 very good
                            2 good
                            3 moderate
                            4 poor
                            5 unsuited
                            0 Not specified