EN AW-1350A

flat bar

A technical illustration of the product with dimensions of the material EN AW-1350A from the material Aluminum in the shape flat bar
  • Form flat bar
  • Material Aluminum
  • Material EN AW-1350A
  • Material chemically EN 573-3 E Al99,5 (A)
  • DIN 3.0257

No product available for your selection.

An image of the material EN AW-1350A from the material Aluminum in the shape flat bar
A technical illustration of the product of the material EN AW-1350A from the material Aluminum in the shape flat bar

Areas of application

Electro-technology

Features of this material

  • Very good welding properties
  •  Very good corrosion resistance to a normal atmosphere 
  •  Very high electrical conductivity as well as thermal 

Features of this material

  • conductivityVery good anodising properties, also decorative
  •  Very good malleability

Information about the material

  • Aviation
    Aviation No
  • Chemical specifications
    Cu (to) 0.02
    Fe (to) 0.4
    Mg (to) 0.05
    Other 0,03
    Rest Aluminium mind. 99,5
    Si (to) 0.25
    Zn (to) 0.05
    0,03 Cr+Mn+Ti+V
  • Chemical surface treatment
    Anodise - decorative 2
    Anodising - protective anodising 1
    Chromating 2
    Cleaning / degreasing 2
    Hard anodising 2
    Phosphating 2
    Pickling 2
    Shining 1
    special anodising quality EQ 1
  • Corrosion resistance
    Normal atmosphere 2
    Seawater atmosphere 3
  • Cutting
    Laser cutting 2
    Plasma cutting 3
    Sawing 4
    Shear cutting 2
    Waterjet cutting 1
  • Food industry
    suitable according to DIN EN 602 Yes
  • Forming
    Bending 1
    Deep drawing (conditional) 1
    Deep drawing conditions H14
    Drop forging 1
    Extruding 1
    Impact extrusion 1
    Press 1
    Upsetting (Conditional) 1
    Upsetting conditions H12
  • Heat treatment - Softannealing
    Heating time max. 2 h
    Heating time min. 0.5 h
    Annealing temperature max. 360 °C
    Annealing temperature min. 340 °C
    Cooling conditions uncontrolled
  • Machining / Machinability
    cold worked 3
    dimensional stability 1
    Eroding 1
    Etching 2
    hardened 4.5
    Photo etching 2
    soft annealed 4.5
  • Material
    Material chemically EN 573-3 E Al99,5 (A)
    DIN 3.0257
    DIN (old designation) E-Al 99,5 A
    France AFNOR -
    Italy UNI 9001/5
    Norway 17,011
    Spain -
    Sweden -
    United Kingdom BS -
  • Mechanical surface treatment
    Blasting 1
    Brushing 3
    Dessinating 1
    Grinding 3
  • Metallic coating
    Galvanising 2
    Nickel coating 1
    Thermal spraying 3
  • Organic coating
    Enamelling 1
    Laminating 2
    Painting / Coating 1
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 23.5 K⁻¹10⁻⁶
    Density 2.7 g/cm³
    Electrical conductivity max. 35.5 m/Ω*mm²
    Electrical conductivity min. 34.5 m/Ω*mm²
    Modulus of elasticity 70 GPa
    Specific heat 900 J/(kg·K)
    Thermal conductivity min. 230 W/m*K
  • Soldering
    Brazing 1
    Brazing with flux 1
    Friction soldering 1
    Soft soldering 1
    Soft soldering with flux 1
  • Welding
    Friction stir welding 2
    Friction welding 2
    Gas 2
    Laser 2
    MIG 3
    Resistance spot welding 4.5
    TIG 2
  • Aviation
    Aviation No
  • Chemical specifications
    Cu (to) 0.02
    Fe (to) 0.4
    Mg (to) 0.05
    Other 0,03
    Rest Aluminium mind. 99,5
    Si (to) 0.25
    Zn (to) 0.05
    0,03 Cr+Mn+Ti+V
  • Chemical surface treatment
    Anodise - decorative 2
    Anodising - protective anodising 1
    Chromating 2
    Cleaning / degreasing 2
    Hard anodising 2
    Phosphating 2
    Pickling 2
    Shining 1
    special anodising quality EQ 1
  • Corrosion resistance
    Normal atmosphere 2
    Seawater atmosphere 3
  • Cutting
    Laser cutting 2
    Plasma cutting 3
    Sawing 4
    Shear cutting 2
    Waterjet cutting 1
  • Food industry
    suitable according to DIN EN 602 Yes
  • Forming
    Bending 1
    Deep drawing (conditional) 1
    Deep drawing conditions H14
    Drop forging 1
    Extruding 1
    Impact extrusion 1
    Press 1
    Upsetting (Conditional) 1
    Upsetting conditions H12
  • Heat treatment - Softannealing
    Heating time max. 2 h
    Heating time min. 0.5 h
    Annealing temperature max. 360 °C
    Annealing temperature min. 340 °C
    Cooling conditions uncontrolled
  • Machining / Machinability
    cold worked 3
    dimensional stability 1
    Eroding 1
    Etching 2
    hardened 4.5
    Photo etching 2
    soft annealed 4.5
  • Material
    Material chemically EN 573-3 E Al99,5 (A)
    DIN 3.0257
    DIN (old designation) E-Al 99,5 A
    France AFNOR -
    Italy UNI 9001/5
    Norway 17,011
    Spain -
    Sweden -
    United Kingdom BS -
  • Mechanical surface treatment
    Blasting 1
    Brushing 3
    Dessinating 1
    Grinding 3
  • Metallic coating
    Galvanising 2
    Nickel coating 1
    Thermal spraying 3
  • Organic coating
    Enamelling 1
    Laminating 2
    Painting / Coating 1
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 23.5 K⁻¹10⁻⁶
    Density 2.7 g/cm³
    Electrical conductivity max. 35.5 m/Ω*mm²
    Electrical conductivity min. 34.5 m/Ω*mm²
    Modulus of elasticity 70 GPa
    Specific heat 900 J/(kg·K)
    Thermal conductivity min. 230 W/m*K
  • Soldering
    Brazing 1
    Brazing with flux 1
    Friction soldering 1
    Soft soldering 1
    Soft soldering with flux 1
  • Welding
    Friction stir welding 2
    Friction welding 2
    Gas 2
    Laser 2
    MIG 3
    Resistance spot welding 4.5
    TIG 2
  • Aviation
    Aviation No
  • Chemical specifications
    Cu (to) 0.02
    Fe (to) 0.4
    Mg (to) 0.05
    Other 0,03
    Rest Aluminium mind. 99,5
    Si (to) 0.25
    Zn (to) 0.05
    0,03 Cr+Mn+Ti+V
  • Chemical surface treatment
    Anodise - decorative 2
    Anodising - protective anodising 1
    Chromating 2
    Cleaning / degreasing 2
    Hard anodising 2
    Phosphating 2
    Pickling 2
    Shining 1
    special anodising quality EQ 1
  • Corrosion resistance
    Normal atmosphere 2
    Seawater atmosphere 3
  • Cutting
    Laser cutting 2
    Plasma cutting 3
    Sawing 4
    Shear cutting 2
    Waterjet cutting 1
  • Food industry
    suitable according to DIN EN 602 Yes
  • Forming
    Bending 1
    Deep drawing (conditional) 1
    Deep drawing conditions H14
    Drop forging 1
    Extruding 1
    Impact extrusion 1
    Press 1
    Upsetting (Conditional) 1
    Upsetting conditions H12
  • Heat treatment - Softannealing
    Heating time max. 2 h
    Heating time min. 0.5 h
    Annealing temperature max. 360 °C
    Annealing temperature min. 340 °C
    Cooling conditions uncontrolled
  • Machining / Machinability
    cold worked 3
    dimensional stability 1
    Eroding 1
    Etching 2
    hardened 4.5
    Photo etching 2
    soft annealed 4.5
  • Material
    Material chemically EN 573-3 E Al99,5 (A)
    DIN 3.0257
    DIN (old designation) E-Al 99,5 A
    France AFNOR -
    Italy UNI 9001/5
    Norway 17,011
    Spain -
    Sweden -
    United Kingdom BS -
  • Mechanical surface treatment
    Blasting 1
    Brushing 3
    Dessinating 1
    Grinding 3
  • Metallic coating
    Galvanising 2
    Nickel coating 1
    Thermal spraying 3
  • Organic coating
    Enamelling 1
    Laminating 2
    Painting / Coating 1
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 23.5 K⁻¹10⁻⁶
    Density 2.7 g/cm³
    Electrical conductivity max. 35.5 m/Ω*mm²
    Electrical conductivity min. 34.5 m/Ω*mm²
    Modulus of elasticity 70 GPa
    Specific heat 900 J/(kg·K)
    Thermal conductivity min. 230 W/m*K
  • Soldering
    Brazing 1
    Brazing with flux 1
    Friction soldering 1
    Soft soldering 1
    Soft soldering with flux 1
  • Welding
    Friction stir welding 2
    Friction welding 2
    Gas 2
    Laser 2
    MIG 3
    Resistance spot welding 4.5
    TIG 2
  • Aviation
    Aviation No
  • Chemical specifications
    Cu (to) 0.02
    Fe (to) 0.4
    Mg (to) 0.05
    Other 0,03
    Rest Aluminium mind. 99,5
    Si (to) 0.25
    Zn (to) 0.05
    0,03 Cr+Mn+Ti+V
  • Chemical surface treatment
    Anodise - decorative 2
    Anodising - protective anodising 1
    Chromating 2
    Cleaning / degreasing 2
    Hard anodising 2
    Phosphating 2
    Pickling 2
    Shining 1
    special anodising quality EQ 1
  • Corrosion resistance
    Normal atmosphere 2
    Seawater atmosphere 3
  • Cutting
    Laser cutting 2
    Plasma cutting 3
    Sawing 4
    Shear cutting 2
    Waterjet cutting 1
  • Food industry
    suitable according to DIN EN 602 Yes
  • Forming
    Bending 1
    Deep drawing (conditional) 1
    Deep drawing conditions H14
    Drop forging 1
    Extruding 1
    Impact extrusion 1
    Press 1
    Upsetting (Conditional) 1
    Upsetting conditions H12
  • Heat treatment - Softannealing
    Heating time max. 2 h
    Heating time min. 0.5 h
    Annealing temperature max. 360 °C
    Annealing temperature min. 340 °C
    Cooling conditions uncontrolled
  • Machining / Machinability
    cold worked 3
    dimensional stability 1
    Eroding 1
    Etching 2
    hardened 4.5
    Photo etching 2
    soft annealed 4.5
  • Material
    Material chemically EN 573-3 E Al99,5 (A)
    DIN 3.0257
    DIN (old designation) E-Al 99,5 A
    France AFNOR -
    Italy UNI 9001/5
    Norway 17,011
    Spain -
    Sweden -
    United Kingdom BS -
  • Mechanical surface treatment
    Blasting 1
    Brushing 3
    Dessinating 1
    Grinding 3
  • Metallic coating
    Galvanising 2
    Nickel coating 1
    Thermal spraying 3
  • Organic coating
    Enamelling 1
    Laminating 2
    Painting / Coating 1
  • physical properties
    Coefficient of thermal expansion from 20 to 100°C 23.5 K⁻¹10⁻⁶
    Density 2.7 g/cm³
    Electrical conductivity max. 35.5 m/Ω*mm²
    Electrical conductivity min. 34.5 m/Ω*mm²
    Modulus of elasticity 70 GPa
    Specific heat 900 J/(kg·K)
    Thermal conductivity min. 230 W/m*K
  • Soldering
    Brazing 1
    Brazing with flux 1
    Friction soldering 1
    Soft soldering 1
    Soft soldering with flux 1
  • Welding
    Friction stir welding 2
    Friction welding 2
    Gas 2
    Laser 2
    MIG 3
    Resistance spot welding 4.5
    TIG 2

1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified