En AW-6012
hexagon bar
- Form hexagon bar
- Material Aluminum
- Material En AW-6012
- Material chemically EN 573-3 AlMgSiPb
- DIN 3.0615
BIKAR Metals companies
Turned parts
Mechanical engineering
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,7 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,3 |
| Cu (to) | 0,1 |
| Fe (to) | 0,5 |
| Mg (from) | 0,6 |
| Mg (to) | 1,2 |
| Mn (from) | 0,4 |
| Mn (to) | 1 |
| Other | max. 0,05 |
| Pb (from) | 0,4 |
| Pb (to) | 2 |
| Rest | Aluminium |
| Si (from) | 0,6 |
| Si (to) | 1,4 |
| Ti (to) | 0,2 |
| Total | max. 0,15 a) b) |
| Zn (to) | 0,3 |
(a) Includes all listed elements for which no limits are specified. (b) The sum of these "other impurities" whose mass fraction is individually 0,010 % or more is expressed with two decimal places before the summation.
| Anodise - decorative | 5 |
| Anodising - protective anodising | 3 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 2 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 1 |
| Normal atmosphere | 2 |
| Seawater atmosphere | 3 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 3 |
| Extruding | 2 |
| Press | 5 |
| Press conditions | T6 |
| Upsetting (Conditional) | 5 |
| Upsetting conditions | T6 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 400 °C |
| Annealing temperature min. | 360 °C |
| Cold ageing condition | danach |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing max. | 16 h |
| Heat ageing min. | 4 h |
| Heating temperature max. | 190 °C |
| Heating temperature min. | 155 °C |
| Solution annealing max. | 530 °C |
| Solution annealing min. | 520 °C |
| Eroding | 1 |
| Etching | 2 |
| hardened | 2 |
| Photo etching | 2 |
| Colorcode | Reinweiß (RAL 9010) |
| Material chemically EN 573-3 | AlMgSiPb |
| DIN | 3,0615 |
| DIN (old designation) | Al Mg Si Pb |
| France AFNOR | A-SG0,5 |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 2,5 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4 |
| Enamelling | 5 |
| Laminating | 2 |
| Painting / Coating | 2 |
| Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
| Density | 2.75 g/cm³ |
| Electrical conductivity max. | 32 m/Ω*mm² |
| Electrical conductivity min. | 24 m/Ω*mm² |
| Modulus of elasticity | 70 GPa |
| Specific heat | 880 J/(kg·K) |
| Thermal conductivity max. | 220 W/m*K |
| Thermal conductivity min. | 170 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 3 |
| Soft soldering | 5 |
| Soft soldering with flux | 5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| MIG | 5 |
| Plasma | 5 |
| Resistance spot welding | 4 |
| TIG | 5 |
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified