EN AW-2011
tube - round as bar
- Form tube - round as bar
- Material Aluminum
- Material EN AW-2011
- Material chemically EN 573-3 Al Cu6 Bi Pb
- DIN 3.1655
Aviation | No |
Be (from) | 0 |
Be (to) | 0 |
Bi (from) | 0.2 |
Bi (to) | 0.6 |
Co (from) | 0 |
Co (to) | 0 |
Cu (from) | 5 |
Cu (to) | 6 |
Fe (to) | 0.7 |
Other | 0,05 |
Pb (from) | 0.2 |
Pb (to) | 0.6 |
Rest | Aluminium |
Si (to) | 0.4 |
Total | 0,15 |
Zn (to) | 0.3 |
0,20 – 0,60 Bi • 0,20 – 0,60 Pb
Anodising - protective anodising | 4.5 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 3 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4.5 |
Normal atmosphere | 4 |
Seawater atmosphere | 5 |
Laser cutting | 4.5 |
Plasma cutting | 4.5 |
Sawing | 1 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | No |
Extruding | 4 |
Impact extrusion conditions | O/H111 |
Upsetting (Conditional) | 3 |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
Cold ageing max. | 8 d |
Cold ageing min. | 5 d |
Heat ageing max. | 16 h |
Heat ageing min. | 8 h |
Heating temperature max. | 185 °C |
Heating temperature min. | 165 °C |
Quenching | water to 65°C/h |
Solution annealing max. | 525 °C |
Solution annealing min. | 515 °C |
Eroding | 1 |
Etching | 2 |
hardened | 1 |
Photo etching | 2 |
Colorcode | Verkehrsrot (RAL 3020) |
Material chemically EN 573-3 | Al Cu6 Bi Pb |
DIN | 3.1655 |
DIN (old designation) | Al Cu Bi Pb |
France AFNOR | A-U5PbBi |
Italy UNI | 9002/5 |
Norway | 17,107 |
Spain | L-3192 |
Sweden | 144,355 |
United Kingdom BS | FC1 |
Blasting | 1 |
Brushing | 2 |
Grinding | 2 |
Polishing | 3 |
Galvanising | 2 |
Nickel coating | 2 |
Thermal spraying | 4 |
Enamelling | 5 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 23.4 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 24 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 21.4 K⁻¹10⁻⁶ |
Density | 2.82 g/cm³ |
Electrical conductivity max. | 32 m/Ω*mm² |
Electrical conductivity min. | 24 m/Ω*mm² |
Modulus of elasticity | 72.5 GPa |
Shear modulus | 27.3 GPa |
Specific heat | 864 J/(kg·K) |
Thermal conductivity max. | 220 W/m*K |
Thermal conductivity min. | 170 W/m*K |
Brazing | 5 |
Brazing with flux | 5 |
Friction soldering | 4 |
Soft soldering | 5 |
Soft soldering with flux | 5 |
Friction stir welding | 5 |
Friction welding | 5 |
Laser | 5 |
MIG | 5 |
Plasma | 5 |
Resistance spot welding | 5 |
TIG | 5 |
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified