EN AW-2007
hexagon bar
- Form hexagon bar
- Material Aluminum
- Material EN AW-2007
- Material chemically EN 573-3 AlCu4PbMgMn
- DIN 3.1645
BIKAR Metals companies
Machine and fixture construction
Turned and milled parts
Screws, nuts
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
| Aviation | No |
| Be (from) | 0 |
| Be (to) | 0 |
| Bi (to) | 0,2 |
| Co (from) | 0 |
| Co (to) | 0 |
| Cr (to) | 0,1 |
| Cu (from) | 3,3 |
| Cu (to) | 4,6 |
| Fe (to) | 0,8 |
| Mg (from) | 0,4 |
| Mg (to) | 1,8 |
| Mn (from) | 0,5 |
| Mn (to) | 1 |
| Ni (to) | 0,2 |
| Other | 0,10 |
| Pb (from) | 0,8 |
| Pb (to) | 1,5 |
| Rest | Aluminium |
| Si (to) | 0,8 |
| Sn (to) | 0,8 |
| Ti (to) | 0,2 |
| Total | 0,30 |
| Zn (to) | 0,8 |
| Anodise - decorative | 5 |
| Anodising - protective anodising | 4,5 |
| Chromating | 2 |
| Cleaning / degreasing | 2 |
| Hard anodising | 3 |
| Phosphating | 2 |
| Pickling | 2 |
| Shining | 4,5 |
| Normal atmosphere | 4,5 |
| Seawater atmosphere | 4,5 |
| Laser cutting | 4,5 |
| Plasma cutting | 4,5 |
| Sawing | 1 |
| Shear cutting | 2 |
| Waterjet cutting | 1 |
| suitable according to DIN EN 602 | No |
| Bending | 4,5 |
| Extruding | 4 |
| Press conditions | O/H111 |
| Upsetting (Conditional) | 4,5 |
| Heating time max. | 2 h |
| Heating time min. | 1 h |
| Annealing temperature max. | 420 °C |
| Annealing temperature min. | 380 °C |
| Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
| Cold ageing max. | 8 d |
| Cold ageing min. | 5 d |
| Heat ageing min. | 16 h |
| Heating temperature min. | 160 °C |
| Quenching | water to 65°C |
| Solution annealing max. | 490 °C |
| Solution annealing min. | 480 °C |
| dimensional stability | 2 |
| Eroding | 1 |
| Etching | 2 |
| hardened | 1 |
| Photo etching | 2 |
| Colorcode | Signalschwarz (RAL 9004) |
| Material chemically EN 573-3 | AlCu4PbMgMn |
| DIN | 3,1645 |
| DIN (old designation) | Al Cu Mg Pb |
| France AFNOR | - |
| Italy UNI | 9002/8 |
| Norway | 17.110 |
| Spain | - |
| Sweden | - |
| United Kingdom BS | - |
| Blasting | 1 |
| Brushing | 2 |
| Grinding | 2 |
| Polishing | 3 |
| Galvanising | 2 |
| Nickel coating | 2 |
| Thermal spraying | 4,5 |
| Enamelling | 4,5 |
| Laminating | 2 |
| Painting / Coating | 4 |
| Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
| Density | 2.85 g/cm³ |
| Electrical conductivity max. | 22 m/Ω*mm² |
| Electrical conductivity min. | 18 m/Ω*mm² |
| Modulus of elasticity | 72.5 GPa |
| Shear modulus | 27.3 GPa |
| Specific heat | 860 J/(kg·K) |
| Thermal conductivity max. | 160 W/m*K |
| Thermal conductivity min. | 130 W/m*K |
| Brazing | 5 |
| Brazing with flux | 5 |
| Friction soldering | 4,5 |
| Friction stir welding | 5 |
| Friction welding | 5 |
| Laser | 5 |
| Plasma | 5 |
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified