EN AW-2007
cast round bar
- Form cast round bar
- Material Aluminum
- Material EN AW-2007
- Material chemically EN 573-3 Al Cu4 Pb Mg Mn
- DIN 3.1645
Aviation | No |
Be (from) | 0 |
Be (to) | 0 |
Bi (to) | 0.2 |
Co (from) | 0 |
Co (to) | 0 |
Cr (to) | 0.1 |
Cu (from) | 3.3 |
Cu (to) | 4.6 |
Fe (to) | 0.8 |
Mg (from) | 0.4 |
Mg (to) | 1.8 |
Mn (from) | 0.5 |
Mn (to) | 1 |
Ni (to) | 0.2 |
Other | 0,10 |
Pb (from) | 0.8 |
Pb (to) | 1.5 |
Rest | Aluminium |
Si (to) | 0.8 |
Sn (to) | 0.8 |
Ti (to) | 0.2 |
Total | 0,30 |
Zn (to) | 0.8 |
Anodise - decorative | 5 |
Anodising - protective anodising | 4.5 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 3 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4.5 |
Normal atmosphere | 4.5 |
Seawater atmosphere | 4.5 |
Laser cutting | 4.5 |
Plasma cutting | 4.5 |
Sawing | 1 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | No |
Bending | 4.5 |
Extruding | 4 |
Press conditions | O/H111 |
Upsetting (Conditional) | 4.5 |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions |
Cooling conditions 30°C/h to 250°C, below 250°C in air |
Cold ageing max. | 8 d |
Cold ageing min. | 5 d |
Heat ageing min. | 16 h |
Heating temperature min. | 160 °C |
Quenching | water to 65°C |
Solution annealing max. | 490 °C |
Solution annealing min. | 480 °C |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
hardened | 1 |
Photo etching | 2 |
Colorcode | Signalschwarz (RAL 9004) |
Material chemically EN 573-3 | Al Cu4 Pb Mg Mn |
DIN | 3.1645 |
DIN (old designation) | Al Cu Mg Pb |
France AFNOR | - |
Italy UNI | 9002/8 |
Norway | 17,110 |
Spain | - |
Sweden | - |
United Kingdom BS | - |
Blasting | 1 |
Brushing | 2 |
Grinding | 2 |
Polishing | 3 |
Galvanising | 2 |
Nickel coating | 2 |
Thermal spraying | 4.5 |
Enamelling | 4.5 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 23 K⁻¹10⁻⁶ |
Density | 2.85 g/cm³ |
Electrical conductivity max. | 22 m/Ω*mm² |
Electrical conductivity min. | 18 m/Ω*mm² |
Modulus of elasticity | 72.5 GPa |
Shear modulus | 27.3 GPa |
Specific heat | 860 J/(kg·K) |
Thermal conductivity max. | 160 W/m*K |
Thermal conductivity min. | 130 W/m*K |
Brazing | 5 |
Brazing with flux | 5 |
Friction soldering | 4.5 |
Friction stir welding | 5 |
Friction welding | 5 |
Laser | 5 |
Plasma | 5 |
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified