EN AW-5083
ring
- Form ring
- Material Aluminum
- Material EN AW-5083
- Material chemically EN 573-3 Al Mg4,5 Mn0,7
- DIN 3.3547
BIKAR Metals companies
Tool making, mould making and model making
Machine and fixture construction
Tank and apparatus construction
Shipbuilding
Automobile components
Railed vehicles
Military technology
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
(a) Includes all listed elements for which no limits are given. (b) The sum of these 'other impurities', the mass fraction of which is individually 0,010 % or more, is expressed with two decimal places before the summation.
Anodise - decorative | 4 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
Laser cutting | 4 |
Plasma cutting | 2 |
Sawing | 3 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 2 |
Deep drawing (conditional) | 2 |
Deep drawing conditions | O |
Drop forging | 4 |
Extruding | 4 |
Impact extrusion | 4 |
Open die forging | 4 |
Press | 4 |
Upsetting (Conditional) | 2 |
Upsetting conditions | O |
Heating time max. | 2 h |
Heating time min. | 1 h |
Annealing temperature max. | 420 °C |
Annealing temperature min. | 380 °C |
Cooling conditions | 30°C/h - 50°C/h |
cold worked | 2 |
dimensional stability | 2 |
Eroding | 1 |
Etching | 2 |
Photo etching | 2 |
soft annealed | 3 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | Al Mg4,5 Mn0,7 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 9005/5 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Blasting | 1 |
Brushing | 2 |
Dessinating | 1 |
Grinding | 2 |
Polishing | 2 |
Galvanising | 2 |
Nickel coating | 1 |
Thermal spraying | 3 |
Enamelling | 3 |
Laminating | 2 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 24.2 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C | 25 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C | 26 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from -50 to 20°C | 22.3 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 19 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 71 GPa |
Shear modulus | 26.8 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Brazing | 4 |
Brazing with flux | 4 |
Friction soldering | 3 |
Soft soldering | 5 |
Soft soldering with flux | 4 |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 3 |
Laser | 2 |
MIG | 2 |
Plasma | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified