FORMODAL® 036 high-strength
ring
- Form ring
- Material Aluminum
- Material FORMODAL® 036 high-strength
- Material chemically EN 573-3 FORMODAL 036-Guss nach Art 7021
- DIN -
Aviation | No |
Anodise - decorative | 5 |
Anodising - protective anodising | 2 |
Chromating | 2 |
Cleaning / degreasing | 2 |
Hard anodising | 2 |
Phosphating | 2 |
Pickling | 2 |
Shining | 4.5 |
Normal atmosphere | 2 |
Seawater atmosphere | 4 |
Laser cutting | 3 |
Plasma cutting | 2 |
Sawing | 1 |
Shear cutting | 2 |
Waterjet cutting | 1 |
suitable according to DIN EN 602 | No |
dimensional stability | 1 |
Eroding | 1 |
Etching | 2 |
hardened | 1 |
Photo etching | 4 |
Material chemically EN 573-3 | FORMODAL 036-Guss nach Art 7021 |
DIN | - |
DIN (old designation) | - |
France AFNOR | - |
Italy UNI | - |
Norway | - |
Spain | - |
Sweden | - |
United Kingdom BS | - |
Blasting | 1 |
Brushing | 2 |
Grinding | 2 |
Galvanising | 2 |
Nickel coating | 2 |
Thermal spraying | 4 |
Enamelling | 5 |
Laminating | 2 |
Coefficient of thermal expansion from 20 to 100°C (typical) | 23.7 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 200°C (typical) | 23.7 K⁻¹10⁻⁶ |
Coefficient of thermal expansion from 20 to 300°C (typical) | 23.7 K⁻¹10⁻⁶ |
Density (typical) | 2.78 g/cm³ |
Electrical conductivity max. (typical) | 23 m/Ω*mm² |
Electrical conductivity min. (typical) | 19 m/Ω*mm² |
Modulus of elasticity (typical) | 72 GPa |
Thermal conductivity min. (typical) | 150 W/m*K |
Friction stir welding | 2 |
Friction welding | 2 |
Gas | 5 |
Laser | 2 |
MIG | 5 |
Plasma | 2 |
Resistance spot welding | 1 |
TIG | 2 |
welding additives |
|
1 very good
2 good
3 moderate
4 poor
5 unsuited