FORMODAL® 024 elox
ring
- Form ring
- Material Aluminum
- Material FORMODAL® 024 elox
- Material chemically EN 573-3 5083
- DIN 3.3547
Aviation | No |
Cr (from) | 0.05 |
Cr (to) | 0.25 |
Cu (to) | 0.1 |
Fe (to) | 0.4 |
Mg (from) | 4 |
Mg (to) | 4.9 |
Mn (from) | 0.4 |
Mn (to) | 1 |
Other | 0,05 |
Rest | Aluminium |
Si (to) | 0.4 |
Ti (to) | 0.15 |
Total | 0,15 |
Zn (to) | 0.25 |
Anodise - decorative | 2 |
Anodising - protective anodising | 1 |
Normal atmosphere | 1 |
Seawater atmosphere | 1 |
suitable according to DIN EN 602 | Yes |
Bending | 5 |
Deep drawing (conditional) | 5 |
Impact extrusion | 5 |
Press | 5 |
Upsetting (Conditional) | 5 |
dimensional stability | 1 |
Eroding | 1 |
Colorcode | Signalbraun (RAL 8002) |
Material chemically EN 573-3 | 5,083 |
DIN | 3.3547 |
DIN (old designation) | Al Mg4,5 Mn |
France AFNOR | A-G4,5MC |
Italy UNI | 7,790 |
Norway | 17,215 |
Spain | L-3321 |
Sweden | 144,140 |
United Kingdom BS | N8 |
Polishing | 2.5 |
Painting / Coating | 4 |
Coefficient of thermal expansion from 20 to 100°C | 23.5 K⁻¹10⁻⁶ |
Density | 2.66 g/cm³ |
Electrical conductivity max. | 18 m/Ω*mm² |
Electrical conductivity min. | 16 m/Ω*mm² |
Modulus of elasticity | 70 GPa |
Specific heat | 900 J/(kg·K) |
Thermal conductivity max. | 140 W/m*K |
Thermal conductivity min. | 110 W/m*K |
Gas | 4 |
MIG | 2 |
Resistance spot welding | 2 |
TIG | 2 |
welding additives |
|
1 very good
2 good
3 moderate
4 poor
5 unsuited
0 Not specified